Stoneware for slow mornings.
Every piece is thrown, trimmed and glazed by hand, then fired for twelve hours to 1285 °C. Choose a glaze, set your table, and we'll make it for you.
- Made to order
- 3–4 weeks
- Fired to
- 1285 °C, cone 10
- Safe in
- Oven, microwave, dishwasher
Set the table before you order it.
Pick a surface, how many people you're feeding and a glaze for each piece. Click any piece on the table to try the next glaze.
Drawn to scale on a 180 × 112 cm table
Total
Made to order in your glazes and shipped in 3–4 weeks.
Four glazes, mixed in the studio.
Each recipe has been tuned over hundreds of test tiles. They all move a little in the kiln, so no two pieces come out the same.
Two weeks from clay to table.
Six steps, all by hand, in one two-room studio. Most of the time is spent waiting: for clay to stiffen, for pots to dry, for the kiln to cool.
Inside one glaze firing
Move along the curve to follow the kiln hour by hour.
The pieces.
Sold one at a time or as a whole table. Every piece carries our stamp on the foot.